1

Topic: Printing problem

hi,

Please advice what is the problem of my printing, please refer to attachment

I use PLA, the wall is 2mm, but the filament not joining.

Please advice

Post's attachments

C360_2014-09-18-19-36-05-964.jpg
C360_2014-09-18-19-36-05-964.jpg 874.48 kb, file has never been downloaded. 

C360_2014-09-18-19-36-23-608.jpg
C360_2014-09-18-19-36-23-608.jpg 801.97 kb, file has never been downloaded. 

C360_2014-09-18-19-37-10-467.jpg
C360_2014-09-18-19-37-10-467.jpg 1.3 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: Printing problem

wheres the infil? is it turned off in slicer? need at min 15% I use 30 on most settings

Solidoodle 2 with Deluxe kit cover & glass bed with heater. and 2nd board SD2 used not 3rd and alum platform not installed yet still wood. also need cooling fan installed to board. use Repetier Host couple vers. Slic3r also have all free ware STL programs

3

Re: Printing problem

Have you done the extruder calibration yet?

SD2 - Glass Bed, Fans on PCB and Y motor, Custom enclosure
Slicer - Simplify3D

4

Re: Printing problem

wire10ga wrote:

Have you done the extruder calibration yet?

+1

These should help you:

http://solidoodletips.wordpress.com/201 … libration/

http://solidoodletips.wordpress.com/201 … flow-rate/

http://www.soliforum.com/topic/2962/dis … p-filling/
Note that relating to this last link, if you are using a .4mm nozzle, the extruded strand width should be around 0.48mm...

SD2 - Stock - Enclosure - Heated Bed - Glass Plate - Auto Fire Extinguisher
Ord Bot Hadron - RAMPS 1.4 - Bulldog XL - E3D v6 - 10" x 10" PCB Heated Build w/SSR - Glass Plate
Thanks for All of Your Help!

5

Re: Printing problem

Dear All,

thank you very much for valuable advice. i will try all the advices.

for sure, i had already calibrated the extruder. but some suggestion still not yet try.

thank you