jooshs wrote:3Dprintergear wrote:Hi jooshs,
I think it will stick fine to ABS, but I will give it a try later today or tonight.
Any chance to try the PVA and sticking it to ABS?
Sorry, I'll get to it soon. Just have some repairs to do first. 8-( Hopefully later today.
OK, I have a print running now that started off with PVA as the raft and have now swapped over to ABS for the rest. ABS had no problems sticking to it, which didn't surprise me as the PVA is quite soft and very sticky feeling. If you leave a thread out in the air after a few minutes you can feel it become tacky.
This will be quite interesting to see how it turns out. I'm sure it will peel away, but if it doesn't then I can just wash it off!