Topic: Solidoodle 3 - Stops extruding after first 20 layers or so
Ok, I'm getting very frustrated with my printer..I have been trying relentlessly to get back to where I can print objects again, and to no avail. I need help please. ![]()
I recently replaced the hot end with another standard solidoodle hot end. My original had a bad clog, when I attempted unscrewing the nozzle from the barrel, the barrel threads broke off inside the nozzle. However, I was experiencing the same problem this post is in regards to with the old hot end as well.
Whenever I print something, the first few layers come out ok. Somewhere between 2-6 mm of height off the build plate, the filament stops sticking to itself. I go to sleep or come home from work, and find the print head moving in mid air above the build plate, with no filament extruding from the hot end, the filament in the extruder stripped completely, the extruder motor full of filament dust...and sometimes, a mushroom shaped clog at the top of the PEEK that prevents me from reversing the filament out of the extruder.
I've tried running at 192 - 205 degrees with the same results every time. Does anyone know what could be the cause? Taking apart the extruder to "fix" these issues, with no successful prints resulting, is getting very tiring.