1

Topic: Trying to calibrate, are these the bust numbers I'm going to get?

I made an L calibration helper.  100mm long X by 100mm long Y, 5mm stand out in the middle of the 100 and 5 mm tall.  these are the numbers im getting when i measure with a caliper.   Can i get better numbers somehow or is this as close as im going to get from an sd3?


http://i5.photobucket.com/albums/y180/Masurrao/EEPROMCalibration.jpg

Overkill is underrated!!!

2

Re: Trying to calibrate, are these the bust numbers I'm going to get?

Did you get your flow rate dialed in perfectly first?  If your perimeters are too wide or thin it will affect the dimensions.   Also watch out for ribbing,  misaligned layers and corner blobs when making measurements since those can make a difference when you get down to tenths of a mm.

3

Re: Trying to calibrate, are these the bust numbers I'm going to get?

i have the extruder almost perfect.  set to .42 mm.   Getting .41 to .43.  I believe when you say ribbing your referring to the backlash of the z?  If so yes i have the spring loaded anti backlash nut installed (was actually impressed at how well that worked).  I don't think misaligned layers are an issue, straight walls look pretty good.   i am getting some corner blobs though.    How does one get rid of those?

Overkill is underrated!!!