Topic: Anyone else have this prob?
I finally got through the little things like extruder clogging, not sticking, etc., and now have a problem that makes no sense to me.
After printing for about 3 hrs filament stops extruding. Spool is on a makeshift holder with little tension or resistance. Tensioner is set adequately, (printed well for 3 hrs +-). Getting good layers and table adhesion.
Anyone have any ideas??