Topic: printBIG - not woriking 4 me...
hey,
after a few weeks of "trail and error" i figured out how to get good results out of my solidoodle3 printer.
but… only in tiny prints…
I tried to print a bigger part (ca. 15cm x 15cm x 15cm) with absolutely no luck… [pictures]
because of the abs tension the layers begin to bent…
I tried a lower extruder temperature – about 190 C
I was thinking: lower temp -> less temp difference -> less tension…
the result was fail.jpg
how can this be done?
can I only print thin and high by changing to pla? or can't this be done anyway?
peet