that doesn't look like z-wobble. That looks like moire from the extruder. Try backing the trimpot on your extruder stepper driver counter clockwise a 1/16-1/32 of a turn.
Other methods for setting extruder trim pot -
[*]set to 0 - full counter clockwise (careful not to go past stop)[/*]
[*]in RH set manual extrude speed to 5mm/s[/*]
[*]extrude 100mm [/*]
[*]slowly adjust the trimpot clockwise (1/16 of a turn at a time) until you hear the extruder start extruding smoothly[/*]
SD3 w/ mods:
Glass bed with QU-BD heat pad upgrade, threadless ballscrew w/ 8mm smooth rod, spectra line belt replacement, lawsy MK5 extruder, Lawsy replacement carriage, E3D hotend, Ramps 1.4 w/ reprap discount controller, DRV8825 drivers, 12v 30A PS, Acrylic case, Overkill Y-idlers, Filament alarm, Extruder fan + more.