Hi everyone,
I've been having issues with my layers sticking to each other.
My bed temp was 105 and my nozzle was at 208.
The print was very brittle and easily broken.
I've attached all my settings that I had for the part which I was trying to print at
.2mm layer height
The bed and nozzle were adjusted manually so it doesn't match the slicer settings