<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Layers not sticking to layers]]></title>
		<link>https://www.soliforum.com/topic/3566/layers-not-sticking-to-layers/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/3566/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Layers not sticking to layers.]]></description>
		<lastBuildDate>Sat, 17 Aug 2013 21:12:50 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Layers not sticking to layers]]></title>
			<link>https://www.soliforum.com/post/33330/#p33330</link>
			<description><![CDATA[<p>Change &quot;infill every&quot; to 1. Layers work best when they are right on top of each other as opposed to having a space in between each one.<br />Try rectilinear infill. Honeycomb may not work to well on something that thin.<br />Are you really using 3mm filament? Have you done any extruder / flow calibration?</p>]]></description>
			<author><![CDATA[null@example.com (FatalDischarge)]]></author>
			<pubDate>Sat, 17 Aug 2013 21:12:50 +0000</pubDate>
			<guid>https://www.soliforum.com/post/33330/#p33330</guid>
		</item>
		<item>
			<title><![CDATA[Re: Layers not sticking to layers]]></title>
			<link>https://www.soliforum.com/post/33143/#p33143</link>
			<description><![CDATA[<div class="quotebox"><cite>techbuilder2175 wrote:</cite><blockquote><p>Does the temp exceed what the extruder from solidoodle is capable of?</p><p>What temps does this black abs need 235?</p></blockquote></div><br /><p>To get 235C on a solidoodle you set the temperature to <strong>205C</strong> as solidoodle reads 30 degrees lower than actual.</p>]]></description>
			<author><![CDATA[null@example.com (ronsii)]]></author>
			<pubDate>Fri, 16 Aug 2013 03:09:05 +0000</pubDate>
			<guid>https://www.soliforum.com/post/33143/#p33143</guid>
		</item>
		<item>
			<title><![CDATA[Re: Layers not sticking to layers]]></title>
			<link>https://www.soliforum.com/post/33101/#p33101</link>
			<description><![CDATA[<p>Does the temp exceed what the extruder from solidoodle is capable of?</p><p>What temps does this black abs need 235?</p>]]></description>
			<author><![CDATA[null@example.com (techbuilder2175)]]></author>
			<pubDate>Thu, 15 Aug 2013 19:24:00 +0000</pubDate>
			<guid>https://www.soliforum.com/post/33101/#p33101</guid>
		</item>
		<item>
			<title><![CDATA[Re: Layers not sticking to layers]]></title>
			<link>https://www.soliforum.com/post/33098/#p33098</link>
			<description><![CDATA[<p>There are a bunch of posts about this particular filament but here&#039;s the wrap up. That black filament from SD needs to be printed at a higher temp. That is the most common filament when people post layer adhesion problems.</p>]]></description>
			<author><![CDATA[null@example.com (2n2r5)]]></author>
			<pubDate>Thu, 15 Aug 2013 19:10:59 +0000</pubDate>
			<guid>https://www.soliforum.com/post/33098/#p33098</guid>
		</item>
		<item>
			<title><![CDATA[Re: Layers not sticking to layers]]></title>
			<link>https://www.soliforum.com/post/33081/#p33081</link>
			<description><![CDATA[<p>Have you ever had success with this filament before?</p><p>As in (my sentence was awkwardly worked), have you used *this specific roll of filament* before with success?</p><br /><p>Sometimes it&#039;s the filament, but I haven&#039;t looked closely at your files and just wanted to see if it warrants further exploration (if you have had success with this filament, it&#039;s probably not the filament. It doesn&#039;t really develop problems part-way through the print.)</p><p>Typically, as far as I&#039;ve seen, inter-layer adhesion is an issue of warping stressing pealing it up (exasperated by thin walls), or bad filament.</p><br /><p>Edit; Do you find those files work better than a razor? I&#039;ve always peeled my prints up with a layer, so I&#039;m curious what your success has been.</p>]]></description>
			<author><![CDATA[null@example.com (Tomek)]]></author>
			<pubDate>Thu, 15 Aug 2013 17:19:05 +0000</pubDate>
			<guid>https://www.soliforum.com/post/33081/#p33081</guid>
		</item>
		<item>
			<title><![CDATA[Re: Layers not sticking to layers]]></title>
			<link>https://www.soliforum.com/post/33074/#p33074</link>
			<description><![CDATA[<p>Here&#039;s the slicer settings</p>]]></description>
			<author><![CDATA[null@example.com (techbuilder2175)]]></author>
			<pubDate>Thu, 15 Aug 2013 16:46:45 +0000</pubDate>
			<guid>https://www.soliforum.com/post/33074/#p33074</guid>
		</item>
		<item>
			<title><![CDATA[Layers not sticking to layers]]></title>
			<link>https://www.soliforum.com/post/33072/#p33072</link>
			<description><![CDATA[<p>Hi everyone,</p><p>I&#039;ve been having issues with my layers sticking to each other. <br />My bed temp was 105 and my nozzle was at 208.<br />The print was very brittle and easily broken.</p><p>I&#039;ve attached all my settings that I had for the part which I was trying to print at <br />.2mm layer height<br />The bed and nozzle were adjusted manually so it doesn&#039;t match the slicer settings</p>]]></description>
			<author><![CDATA[null@example.com (techbuilder2175)]]></author>
			<pubDate>Thu, 15 Aug 2013 16:45:17 +0000</pubDate>
			<guid>https://www.soliforum.com/post/33072/#p33072</guid>
		</item>
	</channel>
</rss>