Topic: Wont Stop Heating
My extruder won't stop heating up. I have it set at 195, and it gets over 220. It has already melted the peek pipe. I have a spare hot end but I don't want to put it in until it stops heating past the setting.
Any ideas?
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Help/Repair/Maintenance → Wont Stop Heating
My extruder won't stop heating up. I have it set at 195, and it gets over 220. It has already melted the peek pipe. I have a spare hot end but I don't want to put it in until it stops heating past the setting.
Any ideas?
For me it was a bad mosfet. I switch the ones for the bed and the hotend on the board since they are the same mosfet.
http://www.soliforum.com/topic/2399/hot … down-320c/
which part is the Mosfet? Where would i get one of those?
https://www.sparkfun.com/products/10213
I fixed my melted peek with a 6mm helicoil from an auto parts store.
Thanks it's working now.