Topic: (SD4)Very messy prints... Possibly my settings?
Greetings,
So with LOTS of help from the soliforum community, I was able to upgrade my SD4 with the E3D lite6. After a few hiccups, its finally printing again, but very sloppy prints. I have been trying to fine tune it for a few days now with no sign of progress. I'm far from professional, so any help would be much appreciated.
So I just printed a 20mm box with ABS. My brim looks really good, just a bit bumpy see from the top view of the brim. But the thing I notice most is that my nozzle drags (scars as its called in the sticky trouble shoot thread) also when it stops to move to a new location, it keep extruding a bit.
I did calibrate how much it extrudes and is extruding 100mm when I hit 100mm in manual control. I also tried to play around 5degrees down because I read it might be too hot.
I also have gaps in the left corner on almost every layer, but Im guessing its from that extra extruded when it stops to move to the next location.
Those two are the main things I noticed just by watching it print. Idk if my settings might need adjusting or not. But here are my settings I used to print the box
The things I adjusted so far was:
Level the bed
adjust my Z stop
adjust the correct amount it being extruded (100mm test)
adjust extruder heat from 210 to 185 in increments of 5degrees
I have a pet bird and I think he will like it better if I print in PLA, but I want to print the fan duct and get all the other settings right before changing from ABS to PLA. And I read that PLA can sometimes be easier than ABS, as lifting is a bad issue I always had.
[edit]
Idk if it says but Im using a .4mm nozzle