Topic: Help with curling edges PLA
I just got my duct fan hooked up using this duct:
http://www.soliforum.com/topic/182/nozzle-fan-duct/
Hooked it up because i was having a lot of trouble with curling edges on small corners and overhangs, but it dosent seem to help that much...i set up a box fan on low about 6ft away from it and that seems to help too. Anything without an overhang comes out nice.
this is what im currently trying to print:
http://www.thingiverse.com/thing:21398
Ive oriented the balls so that a flat side is on the bottom to help. No support.
Most of my problems are happening on the first 20 layers or so, after that the print looks great.
Im wondering what i can do to make the bottom layers look better.
here are my settings.