		<title><![CDATA[SoliForum - 3D Printing Community — Help with curling edges PLA]]></title>
		<link>https://www.soliforum.com/topic/13096/help-with-curling-edges-pla/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/13096/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Help with curling edges PLA.]]></description>
		<lastBuildDate>Wed, 16 Dec 2015 18:31:16 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Help with curling edges PLA]]></title>
			<link>https://www.soliforum.com/post/111792/#p111792</link>
			<description><![CDATA[<div class="quotebox"><cite>TinkerT wrote:</cite><blockquote><p>Oh snap i didnt realize i could just type in a number....</p></blockquote></div><p>No worries! I had the same issue with infill percents, kept wondering how people would print infill that wasn&#039;t divisible by 5... <img src="https://www.soliforum.com/img/smilies/tongue.png" width="15" height="15" alt="tongue" /></p>]]></description>
			<author><![CDATA[null@example.com (widespreaddeadhead)]]></author>
			<pubDate>Wed, 16 Dec 2015 18:31:16 +0000</pubDate>
			<guid>https://www.soliforum.com/post/111792/#p111792</guid>
		</item>
		<item>
			<title><![CDATA[Re: Help with curling edges PLA]]></title>
			<link>https://www.soliforum.com/post/111789/#p111789</link>
			<description><![CDATA[<p>Oh snap i didnt realize i could just type in a number....</p>]]></description>
			<author><![CDATA[null@example.com (TinkerT)]]></author>
			<pubDate>Wed, 16 Dec 2015 17:55:08 +0000</pubDate>
			<guid>https://www.soliforum.com/post/111789/#p111789</guid>
		</item>
		<item>
			<title><![CDATA[Re: Help with curling edges PLA]]></title>
			<link>https://www.soliforum.com/post/111788/#p111788</link>
			<description><![CDATA[<p>yeah i have that but my only options are 0 (soluable) or 0.2(detachable)</p>]]></description>
			<author><![CDATA[null@example.com (TinkerT)]]></author>
			<pubDate>Wed, 16 Dec 2015 17:54:08 +0000</pubDate>
			<guid>https://www.soliforum.com/post/111788/#p111788</guid>
		</item>
		<item>
			<title><![CDATA[Re: Help with curling edges PLA]]></title>
			<link>https://www.soliforum.com/post/111782/#p111782</link>
			<description><![CDATA[<div class="quotebox"><cite>TinkerT wrote:</cite><blockquote><p>Thanks for the advice! Maybe curling was the wrong term but i think you get the idea. these would have turned out worse if i didnt go in after each layer and push it down with a spatula to level it out again for the next layer. </p><p>also i tried it with support but my support fused with the bottom and i dont see any way to change how close the support is to the part in Repeteir Host.</p></blockquote></div><p>If you&#039;re using Slic3r within RH then there is an option in the Slic3r&gt;Print Settings&gt;Support Material that will change that,&nbsp; mine is called &quot;Contact Z Distance&quot; and I&#039;m running Slic3r 1.2.9</p>]]></description>
			<author><![CDATA[null@example.com (widespreaddeadhead)]]></author>
			<pubDate>Wed, 16 Dec 2015 16:37:35 +0000</pubDate>
			<guid>https://www.soliforum.com/post/111782/#p111782</guid>
		</item>
		<item>
			<title><![CDATA[Re: Help with curling edges PLA]]></title>
			<link>https://www.soliforum.com/post/111780/#p111780</link>
			<description><![CDATA[<p>Thanks for the advice! Maybe curling was the wrong term but i think you get the idea. these would have turned out worse if i didnt go in after each layer and push it down with a spatula to level it out again for the next layer. </p><p>also i tried it with support but my support fused with the bottom and i dont see any way to change how close the support is to the part in Repeteir Host.</p>]]></description>
			<author><![CDATA[null@example.com (TinkerT)]]></author>
			<pubDate>Wed, 16 Dec 2015 16:24:20 +0000</pubDate>
			<guid>https://www.soliforum.com/post/111780/#p111780</guid>
		</item>
		<item>
			<title><![CDATA[Re: Help with curling edges PLA]]></title>
			<link>https://www.soliforum.com/post/111735/#p111735</link>
			<description><![CDATA[<p>I print my PLA items with absolutely NO bed heating.&nbsp; I originally heated the bed to about 60, but experienced curling too.</p>]]></description>
			<author><![CDATA[null@example.com (knowack)]]></author>
			<pubDate>Wed, 16 Dec 2015 07:21:57 +0000</pubDate>
			<guid>https://www.soliforum.com/post/111735/#p111735</guid>
		</item>
		<item>
			<title><![CDATA[Re: Help with curling edges PLA]]></title>
			<link>https://www.soliforum.com/post/111676/#p111676</link>
			<description><![CDATA[<p>This doesn&#039;t look like &quot;curling&quot; to me, in the sense of the print pulling up off the plate. It looks more like difficulty printing the overhang.</p><p>Overhangs are notoriously hard to print. Yes, the fan will help, but they still may be a problem. Try these:</p><p>1.&nbsp; Increase the number of outside perimeters (you have 3 maybe try 4 or 5). This will give a broader base for the next level to stick to.</p><p>2. Go slower at lower temperature (there are some scenarios where going faster actually helps instead, ie. bridging).</p><p>3.&nbsp; Use support material</p><p>Ultimately, at the end of the day you are trying to extruder hot, liquid plastic into thin air, and that can be hard to do.</p>]]></description>
			<author><![CDATA[null@example.com (Morganism)]]></author>
			<pubDate>Tue, 15 Dec 2015 18:47:59 +0000</pubDate>
			<guid>https://www.soliforum.com/post/111676/#p111676</guid>
		</item>
		<item>
			<title><![CDATA[Re: Help with curling edges PLA]]></title>
			<link>https://www.soliforum.com/post/111675/#p111675</link>
			<description><![CDATA[<p>I can&#039;t view the pics at work, but I&#039;ve had this problem with emmett&#039;s gears from thingiverse. Try raising the perimeters and infill if they are low.</p>]]></description>
			<author><![CDATA[null@example.com (widespreaddeadhead)]]></author>
			<pubDate>Tue, 15 Dec 2015 18:45:04 +0000</pubDate>
			<guid>https://www.soliforum.com/post/111675/#p111675</guid>
		</item>
		<item>
			<title><![CDATA[Re: Help with curling edges PLA]]></title>
			<link>https://www.soliforum.com/post/111672/#p111672</link>
			<description><![CDATA[<p><span class="postimg"><img src="http://soliforum.com/i/?eJwzRaZ.jpg" alt="http://soliforum.com/i/?eJwzRaZ.jpg" /></span></p><p><span class="postimg"><img src="http://soliforum.com/i/?kep3tU1.jpg" alt="http://soliforum.com/i/?kep3tU1.jpg" /></span></p>]]></description>
			<author><![CDATA[null@example.com (TinkerT)]]></author>
			<pubDate>Tue, 15 Dec 2015 18:27:41 +0000</pubDate>
			<guid>https://www.soliforum.com/post/111672/#p111672</guid>
		</item>
		<item>
			<title><![CDATA[Help with curling edges PLA]]></title>
			<link>https://www.soliforum.com/post/111671/#p111671</link>
			<description><![CDATA[<p>I just got my duct fan hooked up using this duct:</p><p><a href="http://www.soliforum.com/topic/182/nozzle-fan-duct/">http://www.soliforum.com/topic/182/nozzle-fan-duct/</a></p><p>Hooked it up because i was having a lot of trouble with curling edges on small corners and overhangs, but it dosent seem to help that much...i set up a box fan on low about 6ft away from it and that seems to help too. Anything without an overhang comes out nice.</p><br /><p>this is what im currently trying to print:<br /><a href="http://www.thingiverse.com/thing:21398">http://www.thingiverse.com/thing:21398</a></p><p>Ive oriented the balls so that a flat side is on the bottom to help. No support. <br />Most of my problems are happening on the first 20 layers or so, after that the print looks great. </p><p>Im wondering what i can do to make the bottom layers look better. </p><br /><br /><p>here are my settings. </p><p><span class="postimg"><img src="http://soliforum.com/i/?iH9zyIP.jpg" alt="http://soliforum.com/i/?iH9zyIP.jpg" /></span></p><p><span class="postimg"><img src="http://soliforum.com/i/?WwSFSzm.jpg" alt="http://soliforum.com/i/?WwSFSzm.jpg" /></span></p><p><span class="postimg"><img src="http://soliforum.com/i/?AEI0g4n.jpg" alt="http://soliforum.com/i/?AEI0g4n.jpg" /></span></p>]]></description>
			<author><![CDATA[null@example.com (TinkerT)]]></author>
			<pubDate>Tue, 15 Dec 2015 18:22:03 +0000</pubDate>
			<guid>https://www.soliforum.com/post/111671/#p111671</guid>
		</item>
	</channel>
</rss>