Topic: Taulman 618
Anybody tried this stuff?
http://www.taulman3d.com/index.html
How can we turn the extruder up to the 240-250 needed?
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Solidoodle Discussion → Taulman 618
Anybody tried this stuff?
http://www.taulman3d.com/index.html
How can we turn the extruder up to the 240-250 needed?
The extruder usually runs at least 30 degrees hotter then the setting you make in the control software.
I believe a few people on this forum are trying the taulman nylon.... aFoote I think is one of them????
Yeah I ordered mine, I'm waiting on it to come though.
From what I can tell like ronsii said, our extruder when heated to 195 is equal to a higher temperature, so I'll give it a go heated at around 200 when I get it, and go from there.
I'll make sure to document and show pictures to everyone here when it comes in though!
So what did you guys find out? I'm interested in trying this.
Worked really great, oozed a bit more than I'd like it to. The material was great though, but I didn't have a use for it on normal prints. I printed at about 205, with a fan on constantly. Printing at this temperature allowed the layers to adhere better to each other.
Theres a good extensive thread on both the Taulman 618 and a tiny bit on the new clear 645.