need more info like material, temps, ambient conditions as cold drafts can cause warping in spots being printed when cold air hits area while printing, etc for better help. but looks like some of the issue may be flow restriction.
After this problem (http://www.soliforum.com/topic/8119/how-to-fix-blobs/) , I have been tuning these 3D prints.
ABS 1.75
bed temp - 95
extruder - 200
warm enviroment - 20
nozzle diameter - 0.35 (I´ve already tried 0.42)
extrusion multipler adjusted t0 0.79
steps per mm adjusted E:127.00