1

Topic: Nodules? Lumps? Blobs? AH! THE BLOB! RUN!!

I've tried futzing with just about every setting in slic3r..
Getting rather odd blobs on the sides of prints, curiously it only appears on the outward facing walls if I've got more than one object on the print bed.
Happens with both PLA and ABS so temp isn't the problem. Think I've also ruled out over/under extruding too.
http://i.imgur.com/vurVlol.jpg

Any advice will be repaid in internet points which can be spent at the internet.
tongue

Cheers!

This is a crowd funding thing that I'm running: http://www.gofundme.com/bvi140 It's for pretty selfish reasons tongue

2

Re: Nodules? Lumps? Blobs? AH! THE BLOB! RUN!!

Have you tried a different slicer?

SD2 with E3D, SD Press, Form 1+
Filastruder
NYLON (taulman): http://www.soliforum.com/topic/466/nylon/

3

Re: Nodules? Lumps? Blobs? AH! THE BLOB! RUN!!

Ah...... Nope!
Swapped back down the 1.1.5 and it seems the problem has gone away.
Weird.

Thanks comrade!

This is a crowd funding thing that I'm running: http://www.gofundme.com/bvi140 It's for pretty selfish reasons tongue

4

Re: Nodules? Lumps? Blobs? AH! THE BLOB! RUN!!

What's the internet wink

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions