Topic: Nodules? Lumps? Blobs? AH! THE BLOB! RUN!!
I've tried futzing with just about every setting in slic3r..
Getting rather odd blobs on the sides of prints, curiously it only appears on the outward facing walls if I've got more than one object on the print bed.
Happens with both PLA and ABS so temp isn't the problem. Think I've also ruled out over/under extruding too.
Any advice will be repaid in internet points which can be spent at the internet.![]()
Cheers!