Topic: Bottom of Print Not Flat

I started printing a .42 mm calibration cube to set the filament flow, and I noticed that the bottom of the print is curled upwards slightly. This makes it impossible to calibrate the flow rate, so I was wondering if anyone had experienced this before and had a possible solution.

Here is a picture of the finished print, sorry for the poor quality.

Post's attachments

IMG_6367.JPG 1.32 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.
Solidoodle 4, no modifications (yet!)

2

Re: Bottom of Print Not Flat

Yes. Literally thousands of people have encountered this, it is probably the most common issue in all of 3D printing. Try searching for "curl" or "warp".

3

Re: Bottom of Print Not Flat

Of all the nights to not have my PC.  Raise your bed, increase your bed temp to 105 and enclose the printer.  If you don't have glass with hairspray, get some.

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions