Topic: Bottom of Print Not Flat
I started printing a .42 mm calibration cube to set the filament flow, and I noticed that the bottom of the print is curled upwards slightly. This makes it impossible to calibrate the flow rate, so I was wondering if anyone had experienced this before and had a possible solution.
Here is a picture of the finished print, sorry for the poor quality.