muddtt wrote:I guess my first question is: Is this a normal thing to expect?
If it's not, how do I get rid of it?
I've been messing around with retraction settings. Even tried -0.3 on extra length at restart. Nothing seems to be helping that much. Extrusion and feed rate has been calibrated. Any help would be great. Thanks!
Extruder temp: 195
Latest RH/Slicer
What values have you tried for retraction? When I was using the stock hotend, some filaments required almost 2mm of retraction to stop the blobbing. The other thing that helped was adjusting the temps lower by 2-3C. YMMV
SD3 w/ mods:
Glass bed with QU-BD heat pad upgrade, threadless ballscrew w/ 8mm smooth rod, spectra line belt replacement, lawsy MK5 extruder, Lawsy replacement carriage, E3D hotend, Ramps 1.4 w/ reprap discount controller, DRV8825 drivers, 12v 30A PS, Acrylic case, Overkill Y-idlers, Filament alarm, Extruder fan + more.