Please take a look at the two pictures.This is just a simple .3mm cube print.As you can see 3 sides print perfectly but the fourth
does not.Any ideas?

Post's attachments

TEST324.JPG
TEST324.JPG 1.83 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.
SD3, E3D hotend,linear bearing on x/y axis',pillow block bearing on y conneting rod, ball bearngs on front y axis, fan on y stepper motor.

2

Re: test print

This is where the new layers start, you probably need to turn up the retraction amount in slic3r a bit and also turning off randomize start points would make it easier to clean up.

3

Re: test print

ok thanks, I'll try that

SD3, E3D hotend,linear bearing on x/y axis',pillow block bearing on y conneting rod, ball bearngs on front y axis, fan on y stepper motor.

4

Re: test print

Are you sure you calibrated your extrusion settings correctly?  I went through 3/4 roll of filament before I broke down and calibrated it.  I'd double check those and heat it up a little.

5

Re: test print

ah ah no lol I'll have to do that ,  thanks for the tip. I must have wasted just as much.