Topic: first print curled

I ran a test print and it curled.
the bed is warped and I usec a piece of 3/32 glass but it flexes to bad.
Using Octive fluorescent red filiment
bed temp 85° C
extruder 200° C
printer Enclosed
I have to go with 1/8" glass but do i need to up my bed temp

Post's attachments

2013-02-12 17.49.49.jpg
2013-02-12 17.49.49.jpg 881.24 kb, 1 downloads since 2013-02-13 

You don't have the permssions to download the attachments of this post.
Ultimaker S3.

2

Re: first print curled

Since you are using glass on top of the heated bed you need to check the glass temp.  Those readings are from the aluminum plate so the temp of the glass could be anywhere from 5-10d off.  I would try running bed at 95d and see how that prints.  Some people use hairspray to make it stick to the glass as the plastic doesnt stick well to just glass.

3

Re: first print curled

95deg, hairspray, and enclosed build environment.   Then try again.