... I changed the glass today. Went from plain old window glass to a piece of thicker tempered (old scanner top) glass.
Before I started I was printing ABS @ 210/95 1 skirt & no brim - had to almost pry it off the glass. New glass - 220/98 1 skirt 3 brim, and it doesn't stick worth a hoot. My old bed limits out at about 100 - 105. I could go back to the old window glass, I guess..... I also removed the old Kapton tape, haven't put new on yet - will probably have to readjust all again.
What did I change that mattered so much? Does tempered glass make that much of a difference?
Suggestions greatly appreciated...