Topic: s3d configured ?
hello, I use S3D shoulders and neck not very well printed, how well configured? thank you
attach FFF setup s3d
firmware repetier
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → XYZ Printing DaVinci → s3d configured ?
hello, I use S3D shoulders and neck not very well printed, how well configured? thank you
attach FFF setup s3d
Seems like you are under-extruding a bit...try bumping up your Extrusion Multiplier...
Also, you should do a single-wall calibration cube every time you switch filament.
Seems like you are under-extruding a bit...try bumping up your Extrusion Multiplier...
Also, you should do a single-wall calibration cube every time you switch filament.
I have 1,0 I need to increase maximum how much?
1.10 works well for me.
First of all, your Extrusion Width is set to 0.50...it should be 0.48; then follow the steps outlined here:
https://solidoodletips.wordpress.com/20 … flow-rate/
The above was done for a 0.35 dia. nozzle, but the calculations / adjustment procedures are the same...