1 (edited by RandomloserDK 2015-05-14 07:37:15)

Topic: Ugly prints after E3D upgrade.

Hi.
I've upgraded my SD4 with a E3D v6, and updated the firmware to reflect that.
But my prints looks like this:
http://www.soliforum.com/misc.php?action=pun_attachment&item=8668&download=0
http://www.soliforum.com/misc.php?action=pun_attachment&item=8669&download=0

I can't figure out what's causing this.
Can anyone help?

Post's attachments

DSCI0001_v2.JPG
DSCI0001_v2.JPG 96.52 kb, file has never been downloaded. 

DSCI0002_v2.JPG 86.24 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: Ugly prints after E3D upgrade.

too small an area while trying to print, causes previous layers to re-melt.  Try adding another part beside this one or a small column the same height next to this on or speed up last few layers, or add cooling fan.

SD2 - Glass Bed, Fans on PCB and Y motor, Custom enclosure
Slicer - Simplify3D

3

Re: Ugly prints after E3D upgrade.

wire10ga wrote:

too small an area while trying to print, causes previous layers to re-melt.  Try adding another part beside this one or a small column the same height next to this on or speed up last few layers, or add cooling fan.

Thanks I'll try making a pillar somewhere on the bed.

4

Re: Ugly prints after E3D upgrade.

You could also just slide the feedrate slider down when you get to that area of the print.

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions

5

Re: Ugly prints after E3D upgrade.

+1 on all options - consider them an arsenal against melting; you can do a combination of feedrate, tower and fan if you like, they'll all work together.

* Reducing feedrate will only work down to a certain point: eventually the nozzle will remelt locally anyway
* The tower is a bit of a waste of filament but they work well (I did this a lot, including for this exact print, before installing a  fan)
* A nozzle fan brings your useable layer size range down a whole lot, but you sometimes still have to consider the above methods.

The rest of your print looks really tidy from an extrusion point of view. Hang onto those settings!

Next up will be cleaning up that horizontal striping (banding) - check out bed stabilisers and fine-thread z-rods for your next mod! smile

SD3. Mk2b + glass, heated enclosure, GT2 belts, direct drive y shaft, linear bearings, bowden-feed E3D v5 w/ 0.9° stepper