Topic: pictures of my prints, what do you guys think is the problem?
Hi guys,
i was getting great prints with my solidoodle 3.
i had to move from usa to turkey 2 months ago so i put my machine in a shipping container, with great packaging, and it spent 2 months on a cargo ship.
as usual i started to calibrate when i got my hands on it.
I messed up at some point but since i didnt spend time with it for a while, i cant figure it out.i am uploading some pictures so you guys can see the results. I ll also upload my glass bed thickness. It might be too thick. I have my original 0.4 mm nozzle ( i emailed back a lot with solidoodle, they werent sure if they sent me 0.35 or 0.4 but at last they decided it is 0.4mm)
the print was 1.75mm abs, 220 c extruder 120c bed, 3mm layer height, 30% infill no support vs vs.
i lll upload all the settings in a sec.
i am also using the same abs filament that i shipped with my printer. Maybe the humidity also affected it.
here are the pics.
sorry about my english btw.