Topic: calibration issues?
I am trying very hard to get my SD4 dialed in correctly, and it is proving to be a bit of a challenge... I have done a LOT of searching, reading, and learning since it arrived.
first off, this thing was puchased used, and when it arrived it had some adjusting that needed to be done - things just were not lined up properly causing a little bit of binding. I think I got that pretty well sorted out, and belts tensioned evenly...i can move the printhead around manually fairly easily now.
have played around with printing various things and getting ok results, but feel they could be better, so I read up on calibrating the flow rate here: http://support.solidoodle.com/hc/en-us/ … alibration
here is where things get interesting...
the very first line (left to right at the front) of the actual cube is off - when it starts to lay down that first solid fill layer, the first line is not met with the fill... I killed the print to snap the first pic...
all layers after that - from 2 on up, lay down just fine and where they are supposed to be. It is ONLY on that very first line. Can be seen in pic 2 as well (sorry for the poor quality - cell phone) of a partially completed cube..
i hadnt really paid much attention to this in previous test cube prints, but it is the same on ALL of them. So - systematic problem, right?
so how do I go about fixing it? Or can I fix it? Belts too tight? too loose? just how tight are they supposed to be anyway?
I am still learning here, so some of the terminology is still a little foreign to me. Please bear with me as I learn...
edit to add: I am using PLA for all of this - easier for me to work with for now...
Stock SD4
Prusa i3 kit, spring loaded extruder upgrade, Y axis belt tensioner