No red, i had too many problems at one time, i wanted to get the excess height and unevenness out of it (take away mk2 for now) to troubleshoot. Wanted as few variables as possible, to eliminate either something I did ie adding MK2 or software or stock part wise.
Good logic.
But I think your putting a bandaid on your extrusion issue with that, not fixing it.
Good logic.
But I think your putting a bandaid on your extrusion issue with that, not fixing it.
Whats the fix!? I thought tinkering settings was
OneMoreCast
Bumped flowrate up, and feedrate down...woohoo
can you screen shot what you changed so i can make sure i am in the right place i have that problem too
OneMoreCast
Bumped flowrate up, and feedrate down...woohoocan you screen shot what you changed so i can make sure i am in the right place i have that problem too
My major problem was I switched to a RUMBA board w 1/32 stepping and my steps per mm where off. Also extruder was calibrated wrong, pretty much everything out of wack. Once all that was dialed in flow and feed stay at 100...as mentioned before its not a solution. When its properly setup both at 100 will work fine. Post pic of your EEPROM numbers from RH
That's suck for me I was Hopping it wAz just a setting so I could get mine dialed in right
Upload your slic3r config file..also have you tried slicing with Cura and printing!?
Cura works but i can not set it to make # 2 Extrude as primer if i want to switch colors
SoliForum - 3D Printing Community → Solidoodle Discussion → SOLVED-Print layers look like Ramen noodles
Powered by PunBB, supported by Informer Technologies, Inc.