26 (edited by redbarret 2015-01-23 07:45:41)

Re: SOLVED-Print layers look like Ramen noodles

I just noticed, where did your mk2 heatbed go?
I hope you're not mistaking MK5 extruder for an MK2 heatbed and thinking of upgrading because of that.

Solidoodle 4

27

Re: SOLVED-Print layers look like Ramen noodles

http://s2.postimg.org/47bu20vvp/image.jpg Bumped flowrate up, and feedrate down...woohoo

"All your base are belong to us." SD4 with a RUMBA, supernight PS, 40mm fan on X motor, lawsey carriages with new better tolerance rods, flanged rear bearings, new NEMA 17 with leadscrew on Z-Axis, and e3d v6 with MK5.


Ward and Jago are my heroes tongue

28 (edited by OneMoreCast 2015-01-23 08:01:21)

Re: SOLVED-Print layers look like Ramen noodles

No red, i had too many problems at one time, i wanted to get the excess height and unevenness out of it (take away mk2 for now) to troubleshoot. Wanted as few variables as possible, to eliminate either something I did ie adding MK2 or software or stock part wise.

"All your base are belong to us." SD4 with a RUMBA, supernight PS, 40mm fan on X motor, lawsey carriages with new better tolerance rods, flanged rear bearings, new NEMA 17 with leadscrew on Z-Axis, and e3d v6 with MK5.


Ward and Jago are my heroes tongue

29

Re: SOLVED-Print layers look like Ramen noodles

Good logic.
But I think your putting a bandaid on your extrusion issue with that, not fixing it.

Solidoodle 4

30

Re: SOLVED-Print layers look like Ramen noodles

redbarret wrote:

Good logic.
But I think your putting a bandaid on your extrusion issue with that, not fixing it.


Whats the fix!? I thought tinkering settings was

"All your base are belong to us." SD4 with a RUMBA, supernight PS, 40mm fan on X motor, lawsey carriages with new better tolerance rods, flanged rear bearings, new NEMA 17 with leadscrew on Z-Axis, and e3d v6 with MK5.


Ward and Jago are my heroes tongue

31 (edited by cpsmicahel 2015-01-29 02:33:16)

Re: SOLVED-Print layers look like Ramen noodles

OneMoreCast
Bumped flowrate up, and feedrate down...woohoo


can you screen shot what you changed so i can make sure i am in the right place i have that problem too

• Solidoodle Workbench Apprentice
• Creates plastic parts up to 6" x 6" x 8"
• Heated Aluminum Build Platform with Glass Bed
• Dual extruder

32 (edited by OneMoreCast 2015-01-29 03:41:09)

Re: SOLVED-Print layers look like Ramen noodles

cpsmicahel wrote:

OneMoreCast
Bumped flowrate up, and feedrate down...woohoo


can you screen shot what you changed so i can make sure i am in the right place i have that problem too


My major problem was I switched to a RUMBA board w 1/32 stepping and my steps per mm where off. Also extruder was calibrated wrong, pretty much everything out of wack. Once all that was dialed in flow and feed stay at 100...as mentioned before its not a solution. When its properly setup both at 100 will work fine. Post pic of your EEPROM numbers from RH

"All your base are belong to us." SD4 with a RUMBA, supernight PS, 40mm fan on X motor, lawsey carriages with new better tolerance rods, flanged rear bearings, new NEMA 17 with leadscrew on Z-Axis, and e3d v6 with MK5.


Ward and Jago are my heroes tongue

33

Re: SOLVED-Print layers look like Ramen noodles

That's suck for me I was Hopping it wAz just a setting so I could get mine dialed in right

• Solidoodle Workbench Apprentice
• Creates plastic parts up to 6" x 6" x 8"
• Heated Aluminum Build Platform with Glass Bed
• Dual extruder

34 (edited by OneMoreCast 2015-01-29 07:57:44)

Re: SOLVED-Print layers look like Ramen noodles

Upload your slic3r config file..also have you tried slicing with Cura and printing!?

"All your base are belong to us." SD4 with a RUMBA, supernight PS, 40mm fan on X motor, lawsey carriages with new better tolerance rods, flanged rear bearings, new NEMA 17 with leadscrew on Z-Axis, and e3d v6 with MK5.


Ward and Jago are my heroes tongue

35

Re: SOLVED-Print layers look like Ramen noodles

Cura works but i can not set it to make # 2 Extrude as primer if i want to switch colors

Post's attachments

Slic3r_config_bundle.ini 16.26 kb, 4 downloads since 2015-01-30 

You don't have the permssions to download the attachments of this post.