I'll put this warping query under this no sticky thread as that is the end result of a solid build warping so much it loses its footing.
It is the base part of the mini shreader that the author suggested to print solid infill.
So I did and it warped badly (bottom left not flat),and this for thick piece of plastic, not some skinny laid out leg, which I would expect to warp. Or is this just temp strinkage?
Why is this? Expect it on large solid builds or is the bed got a temp differential at the front back y axis at the ends of the bed?
I cut the rest of the part in netfabb and printed that with 50 per cent infill and little warping occurred.
The image has somehow got inverted/reflected vertically????
Post's attachmentsimage.jpg
image.jpg 1.6 mb, file has never been downloaded.