Three prints on the same stock 1.0 machine
Filament: Filament Outlet Natural
Extruder Temp: 225
Bed Temp: 80
Unless otherwise indicated all settings are default
pic #1 - Firmware: 1.1.J Slicer: XYZware 1.1.1(mac) Density: 90% Layer Height: .1 Speed: Slow
pic #2 - Firmware: 1.1.J Slicer: 3DSimplify 2.2.1 Infill %: 100 Layer Height: .1 Speed: 1800 mm/min
pic #3 - Firmware: 1.2.3 Slicer: XYZware 1.1.1(mac) Density: 90% Layer Height: .1 Speed: Slow
Post's attachmentsPhoto on 1-9-15 at 6.55 PM #2.jpg
Photo on 1-9-15 at 6.55 PM #2.jpg 147.76 kb, file has never been downloaded.
Photo on 1-9-15 at 6.55 PM.jpg
Photo on 1-9-15 at 6.55 PM.jpg 134.59 kb, file has never been downloaded.
Photo on 1-9-15 at 6.56 PM.jpg
Photo on 1-9-15 at 6.56 PM.jpg 147.08 kb, file has never been downloaded.
You don't have the permssions to download the attachments of this post.