Topic: Slic3r settings for Z-lift?
the
avoid crossing perimeters setting does NOT lift Z (extruder) as many here have posted. all it does is use a defferent path when moving to avoid last layer laid. no Z height changes ever. so it still hits some detail parts knocking them loose.
small parts tend to curl while cooling putting them up into path of extruder.