Topic: Solidoodle 2 Wavey/ blobby prints
Hi all,
Recently my Solidoodle has been printing some wavy lines. It seems to be doing this on both X and Y, so I don't think it's either of these steppers (It'd be unlikely for both to be messed up, right?) . I don't think it's over-extruding, as I've calibrated the extrusion rate, and infills are nice. I've also calibrated and checked Vrefs on all motors, and cleaned and rebuild my extruder (E3D v5). And so I'm stumped on where to go from here.
Attached files,
Third one shows a nice old print. All straight and cool.
Second and first show the problem. Wavey wavey.
Any ideas chaps?