Topic: calibration cube
is the right stl file a complete cube or an open top box? all I found was closed hollow cube and cant get Slic3r to stop making a raft, 10 layers bottom and 2 perimiters no matter how many times I try and reset save re-slice.
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Solidoodle Discussion → calibration cube
is the right stl file a complete cube or an open top box? all I found was closed hollow cube and cant get Slic3r to stop making a raft, 10 layers bottom and 2 perimiters no matter how many times I try and reset save re-slice.
ok found right box and test print came out to .41mm all 4 sides
Normally I use a plain 20mm cube (solid), and instruct slic3r to perform about 2 bottom layers (make sure it sticks...), 0 top layers, just 1 perimeter and 0% infill.
I usually create this profile from my existing normal profile, so it picks up all the other settings identically for a fair comparison!
Normally I use a plain 20mm cube (solid), and instruct slic3r to perform about 2 bottom layers (make sure it sticks...), 0 top layers, just 1 perimeter and 0% infill.
I usually create this profile from my existing normal profile, so it picks up all the other settings identically for a fair comparison!
+1