Ok, so I've done everything I could read about. I've calibrated the extruder, leveled the bed, adjusted the rails and belts, tightened just about everything I could find info on. But my prints are terrible. I've tried different batches of ABS (one freshly opened from an air tight package with a dehumidifier packet included), I've adjusted the temps a bit and just can't seem to find a happy place.
These two that are pictured were printed with the extruder temp at 200 and the bed at 95.
So you guys that have been doing this for a while, what's the first thing that pops into your mind when you see these prints?? Believe it or not, these are the best that's come out of this thing so far and they just crumble when I bend them.
ANY info appreciated. TIA