1

Topic: Unable to reach 250 degrees

I have been printing with PLA since I got the printer, so I set my printer to 210 and that worked out fine. Once I got some ABS, I tried printing at 250. The printer would go fine until it reached 236 and the it would stop and start to drop. I am using a e3d v6 and the original solidoodle board.

Ulitmaker 2, a few repraps, Custom Big FFF 3D printer with heated chamber.

My Blog http://ggalisky.weebly.com/
My Youtube https://www.youtube.com/channel/UCXShYo … aDUpebDAOw

2

Re: Unable to reach 250 degrees

Sounds to me like you never flashed the board like you were supposed to. That also means you've ben running on the wrong thermistor setting.

Good times.

3

Re: Unable to reach 250 degrees

A little toasty for abs IMHO. I run 205-215 (maybe at most 220 to get those layers together) but I'm pretty new still.

Solidoodle 2 Pro - 3mm Glass Bed

4

Re: Unable to reach 250 degrees

exineport wrote:

A little toasty for abs IMHO. I run 205-215 (maybe at most 220 to get those layers together) but I'm pretty new still.

You're using a completely different hotend which measures temperature in a different location.

5

Re: Unable to reach 250 degrees

elmoret wrote:
exineport wrote:

A little toasty for abs IMHO. I run 205-215 (maybe at most 220 to get those layers together) but I'm pretty new still.

You're using a completely different hotend which measures temperature in a different location.

My bad, disregard.

Solidoodle 2 Pro - 3mm Glass Bed

6

Re: Unable to reach 250 degrees

Yep... Make the changes in firmware and then run at 240 - 250 for ABS

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions

7

Re: Unable to reach 250 degrees

Thanks guys! It is all working great.