AZERATE wrote:How is your tension arm? If it is too loose, the bearing (to the right) will not turn at the same pace as the Nema gear. Thus, giving you random voids.
This is one thing I noticed whilst learning my machine.
EDIT: A dead giveaway of this would be stripping of filament in the extruder. This can also be a sign of a clog, but I don;t think this is the case with your problem.
It's not very tight, but not loose enough to skip from what I'm seeing. I'm no sure it's actually gapping anymore, but where the gap is the extrusion is raised, I am actually seeing it when watching.... No grinding or plugs on the extruder, I'm used to handling those issues,
things I've changed, to no effect;
Raised the Extruder reference voltage to 0.355 from 0.192, definitely squirting more out, need to recalibrate... still have the gaps.
Raised the temp from 200 to 215 for the extruder... still gapping....
Slowed down the printer to 50%, standard perimeters were printing at 70mm/s, external perimeters at 35% at normal rate, I changed this during mid print, it seems better, not perfect, but better..... I wouldn't think 70mm/s would be too fast for ABS perimeters?
Wondering if the filament is crap and this could be a result of that? Going to try my roll of orange I got from a different vendor.
Thanks