Topic: Lifting issues on medium sized prints
I slapped on a mirror bed a few months ago and have experimented between different hairsprays, ABS slurry, and even different glues. But it seems anything I print that covers more of the bed refuses to stay put. Most of my designs do not need to be perfect, but I'm trying to get everything printed to upgrade to Lawsy's carriages and it is not going so well.
Above image was printed at .1mm at 65% infill. Feed 100/Flow 95

This part was printed at .2mm at 80% infill and has significantly less warping. I want to say the Feed/Flow were even at 100. Bed temp for both prints was 90c.
I experiment with my settings almost daily and am having fun getting it dialed in, but the inconsistencies of adhesion is making me scratch my head.
Any ideas?
Thanks in advance.
Multiple SD2s- Bulldog XL, E3D v5/v6/Lite6, Volcano, Hobb Goblin, Titan, .9 motor, Lawsy carriages, direct Y drive, fishing line...the list goes on