Topic: Adjusted extruding rate, now infill too low?

Hey, I just posted a question regarding my problems with the too high extrusion rate and I adjusted it.
Now walls are nice, but I have problems with overhangs and Top solid Infill. Looks like there's not enough plastic coming out for the infill. I attached some photos to show the printing results.
David

Post's attachments

Foto 1.JPG
Foto 1.JPG 441.51 kb, file has never been downloaded. 

Foto 2.JPG
Foto 2.JPG 451.21 kb, file has never been downloaded. 

Foto 3.JPG
Foto 3.JPG 480.54 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2 (edited by MolecularConcept 2014-02-18 03:02:15)

Re: Adjusted extruding rate, now infill too low?

how many top layers do you have ? you need at least 3 especially withh a lower infill percentage. and combine infill every 1 layers

3

Re: Adjusted extruding rate, now infill too low?

The problem was that I was just printing too fast.