lawsy wrote:I'm not sure if you've tried hairspray yet but it works wonders.
Hairspray had no affect at all, sadly. I've printed some fairly large things in the past, but suddenly, nothing works.
I have re-leveled the bed (as best I can, since there is a low spot on the far right). It is set so that a piece of paper just barely makes it under the print head for everything but the far right; the paper measures 0.10 mm thick.
Bed is set to 85 degrees, and extruder is at 195.
I've gone from happy production oriented guy to frustrated head scratching guy
I have two glass plates, which I could try to use, but the kapton was working well for a while, and now suddenly parts of it are not.
I put a glass plate on, using springs as clamps (see photo). The glass plate is held in place with a clip on the near right and far left. The depression on the far right is still obvious when using paper. That is, the lack of flatness in the bed is mirrored in the glass. I had not expected this at all
Time to get a new bed, I guess. Frustrating