I just went through this today, as I was having issues. Instead of downloading something from Thingiverse, I made my own test piece that has walls at right angles to each other as well as 45° angles, curves and even a hole in the center to test for roundness.
Here is what the final output looks like after I tweaked the flow rate and the extruder steps.

The stringy things between the cylinder wall and the outer wall was a result of my Retraction setting. I had the "Extra Length on Retract" set to .5mm, after I put it back to 0mm, the little stringy things went away.
I've attached my test model. If you want to print it, set the Vertical Shells: Perimeters to 1, Horizontal Shells: Top Solid Layer to 0, Bottom Layer to 3, and Infill: Fill Density to 0. Slice & print.
You can also use it to calibrate your X & Y steps. The left side is 50mm, the square notch is 10x10mm, from the left corner to the notch it's 20mm, the hole diameter is 20mm, and the height is 10mmm
Post's attachmentscalibration part print.jpg
calibration part print.jpg 1.1 mb, file has never been downloaded.
calibration part.STL 12 kb, 13 downloads since 2014-02-03
You don't have the permssions to download the attachments of this post.
To print or, 3D print, that is the question...
SD3 printer w/too many mods, Printrbot Simple Maker Ed., FormLabs Form 1+
AnyCubic Photon, Shining 3D EinScan-S & Atlas 3D scanners...
...and too much time on my hands.