Topic: Best temperature for printing white pla?
I have an unheated bed and just switched to pla because i stupidly bought abs now whats the best temp for printing white pla ?
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Help/Repair/Maintenance → Best temperature for printing white pla?
I have an unheated bed and just switched to pla because i stupidly bought abs now whats the best temp for printing white pla ?
With the stock Solidoodle hot end, 180 seems to work well for me.
I do 170-180. I experiment. And while I still have my stock featues, I have not noticed much (if any) difference between the temps.
But for printing PLA, you will want a 40mm fan for the hot end. If you are impatient or it is not an option, you can use a simple desk fan, which is what I used to print my fan mount since I print PLA exclusively. PLA takes longer to cool than ABS, so depending on the size of the print or if you have a case built, it is crucial to have a fan while printing PLA.
I AM, however, still finding my niche with PLA filaments. I've tried JustPLA (don't recommend), and Makerbot which has worked best for me. That being said, what brand did you get?