So I took about 300mm of white ABS filament and put it into this glass jar filled with 1/3 full of acetone. Put the jar in hot water for a day. All of the filament dissolved and just a goop right now. But it won't mix with acetone.
The ABS goop and acetone just sit there in 2 layers in that jar.
I poked the goop and it's like tooth paste. Acetone that sit on top is very clear.