1 (edited by Kevin Gossett 2014-01-15 15:26:00)

Topic: Help Me Dial In

So far I have done the following:
- calibrated extruder and flow rate
- glass bed, leveled
- adjusted tension in belts
- acrylic enclosure

I've only printed parts for the enclosure, so I wanted to try something else. I printed the Key to Eribor from The Hobbit off Thingiverse at mostly default settings (.3 mm with support)

Tonight I'm going to bump up the resolution to see what that looks like. Any other suggestions to help me get the most out of my prints?

Post's attachments

20140115_003349.jpg
20140115_003349.jpg 3.71 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: Help Me Dial In

Looks like you are still over extruding.  try dialing back the Extrusion multiplier a little

3

Re: Help Me Dial In

I'll give that a try. Anything else?

4

Re: Help Me Dial In

Adjusted the multiplier. Went from .75 to .70

Printed the key again, scaled slightly up, at .1 mm. Still need to trim some of the brim off in places, and there are definitely artifacts

Post's attachments

20140116_092046.jpg 2.64 mb, file has never been downloaded. 

20140116_092054.jpg
20140116_092054.jpg 1.82 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

5

Re: Help Me Dial In

what temp do you have the extruder set to?

6

Re: Help Me Dial In

Bed at 200, extruder at 100