Topic: Skeinforge (50) help
I have been trying to configure a profile for Skeinforge for my SD3. I have been printing a single wall test square, the same one I used for Slic3r. I have been able to adjust the speed and flow to get the correct wall thickness of .45mm for a .3mm layer height. My problem is it creates a blob of plastic at the start of each level. Slic3r does not do this. What setting can I use to correct this? I have attached a picture.