Topic: stumped with PLA
My Solidoodle 2 pro model runs ABS all day long. I got some PLA food Christmas and it runs OK. I am running it at 185-190C bed temp at 70C. It runs great on nice big geometry but on small geometry it seems like I am not getting enough flow. So I upped my extruder multiplyer back up to 1. Does the trick on small geometry. However large geometry suffers the material starts bulging up and out. I can't seem to find a happy medium. Oh and this is at .100 mm layers. Any thoughts would be appreciated. Thanks.
Curly