Topic: Solidoodle 2 Prints have bumps, gaps
Hi guys,
All of my prints seem to have bumps all over them on every layer change and on the outer perimeter. I don't think retraction is the issue, during the print you can hear it retracting quite aggressively.
.3mm Layer height, gcode looks ok, Slic3r
imgur.com/a/ttlzb
Any help would be appreciated! I am going to try adjusting z tab.