1

Topic: Very ugly artifacts when printing

Appear on the surface with a small reverse bias. Has anyone seen anything similar?
Use Slic3r 1.0.0RC1 and Repetier-Host from last Solidoodle package download.
Thread when printing does not sag, does not fall, it's okay.

Post's attachments

body.jpg 301.4 kb, file has never been downloaded. 

bodyr.jpg
bodyr.jpg 329.39 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: Very ugly artifacts when printing

3d, did you run your stl through Netfab first?

3

Re: Very ugly artifacts when printing

Briggs wrote:

3d, did you run your stl through Netfab first?

Why Netfab? This issue happened with all similar models, directly downloaded from thingiverse, and with my own-maded. For .stl repairing i use Materialize Magics. How Netfab can help me in this case?

4

Re: Very ugly artifacts when printing

The artifacts do not appear in the g-code visualization, so I'd be very surprised if this were the stl or slicers fault.  I've never seen anything like this however, so don't totally rule them out.  Have you seen this behavior on any other prints?

5

Re: Very ugly artifacts when printing

COASTER19 wrote:

The artifacts do not appear in the g-code visualization, so I'd be very surprised if this were the stl or slicers fault.  I've never seen anything like this however, so don't totally rule them out.  Have you seen this behavior on any other prints?

Yes, on the other prints I see the same things. Apparently it began after I switch from the use of Pronterface to the Repetier-Host, it can be?