Topic: Some general guidance needed.
Hello guys having some issues.. I have an SD3. Ive done the calibrations and such and Ive been experimenting with different methods to get filament to stick well. Im getting more successful, but I've run into another problem.
When printing somthing that curves outward from the base, or filling the top of a round hole the filament is not sticking or its dragging away from where it should be. I've tried slowing it down, adding other things to the bed to print because I thought it was just too hot, but the problem persists even at a super slow speed. So Im not sure whats doing it. Here is an example of whats happening. I was trying to print this tic tool, which I have printed before and its worked fine.
thingiverse com/thing:22786
But today the result is this and I cant figure out why...
I cant post links for some reason..
Youtube these:
BeszOeGq3ow
FddqY2HbSnQ
And; A previous print on the right, current try on the left.
i.imgur.com/xMPrldq.jpg
Any help for a noob would be great!
Thanks!