muddtt wrote:Here's my ghetto case mod so far
Even has a hinge with a magnet.
Got lucky at Lowes and picked up 2 clear plastic pieces for $2. He said normally he's allowed to cut and give away scrap for free, but the manager got a little picky. No complaints with $2.
Nice. I just use a Reflectix coozy. Wrap one sheet around the 3 sides and tie it off with jute, and another piece set on top with a "double pane" half a zip lock bag plastic window taped in it. So that is my red neck ghetto rig.
I find I only feel the need to use it for printing a lot of separate pieces that would cool down too much and maybe have delamination problems later. Like all the hubs for this dome in one go for instance. http://www.thingiverse.com/thing:157783